Annotation
Increasing the concentration of indium atoms and hydrogen was found in the $\alpha$-phase of the foil of a Pd-In alloy (with 5.3 and 5.0 at % In) after its electrolytic hydrogenation and 500-h relaxation. It is shown that the structural variations in the foil during the $\alpha\rightarrow\beta$ transformation are nonmonotonic.
Received: 2013 October 23
Approved: 2014 May 23
PACS:
61.10.Nz X-ray diffraction
61.72.Dd Experimental determination of defects by diffraction and scattering
61.72.Ss Impurity concentration, distribution, and gradients
61.50.Ks Crystallographic aspects of phase transformations; pressure effects
61.72.Dd Experimental determination of defects by diffraction and scattering
61.72.Ss Impurity concentration, distribution, and gradients
61.50.Ks Crystallographic aspects of phase transformations; pressure effects
© 2016 Publisher M.V.Lomonosov Moscow State University
Authors
V.M. Avdyukhina, O.V. Akimova, I.S. Levin, G.P. Revkevich
Department of Physics, Moscow State University, Moscow, 119991, Russia
Department of Physics, Moscow State University, Moscow, 119991, Russia